medium
Cold shuts are casting defects
Show Hint
Cold Shut = Poor Fusion. The metal was too "cold" to "shut" (merge) the gap.
AP ECET Metallurgical Eng - 2026
AP ECET Metallurgical Eng
Updated On:
Jul 4, 2026
Which occur due to some sand shearing from the cope surfaces
Which take the form of interval voids or surface depression due to excessive gaseous material not able to escape
Which occur due to discontinuity in metal casting resulting from hindered contraction
Caused by two streams of metals that are too cold to fuse property
Show Solution
The Correct Option is
D
Solution and Explanation
Download Solution in PDF
Was this answer helpful?
0
Top Questions on Casting and Foundry
The impurities in centrifugal casting are
AP ECET Metallurgical Eng - 2025
Metallurgical Engineering
Casting and Foundry
View Solution
Wood flour is added to the moulding sand to improve
AP ECET Metallurgical Eng - 2025
Metallurgical Engineering
Casting and Foundry
View Solution
An expandable pattern is used in
AP ECET Metallurgical Eng - 2025
Metallurgical Engineering
Casting and Foundry
View Solution
The riser is designed such that the melt in the riser solidifies
AP ECET Metallurgical Eng - 2025
Metallurgical Engineering
Casting and Foundry
View Solution
Want to practice more? Try solving extra ecology questions today
View All Questions
Questions Asked in AP ECET Metallurgical Eng exam
Order of the matrix $\begin{bmatrix} 1 & 6 \\ 2 & 0 \\ 7 & -1 \end{bmatrix}$ is
AP ECET ME - 2025
AP ECET ECE - 2025
AP ECET Metallurgical Eng - 2025
AP ECET Mining Engg - 2025
Matrices and Determinants
View Solution
If two rows (or columns) of a determinant of order 3 are identical then the value of determinant is
AP ECET ME - 2025
AP ECET ECE - 2025
AP ECET Metallurgical Eng - 2025
AP ECET Mining Engg - 2025
Matrices and Determinants
View Solution
Co-factor of -4 in $\begin{vmatrix} 1 & 2 & 3 \\ -4 & 3 & 6 \\ 2 & -7 & 9 \end{vmatrix}$ is
AP ECET ME - 2025
AP ECET ECE - 2025
AP ECET Metallurgical Eng - 2025
AP ECET Mining Engg - 2025
Matrices and Determinants
View Solution
The Matrix $\begin{bmatrix} a & h & g \\ h & b & f \\ g & f & c \end{bmatrix}$ is
AP ECET ME - 2025
AP ECET ECE - 2025
AP ECET Metallurgical Eng - 2025
AP ECET Mining Engg - 2025
Matrices and Determinants
View Solution
If $A = \begin{bmatrix} 0 & 0 & 1 \\ 0 & 1 & 0 \\ 1 & 0 & 0 \end{bmatrix}$ then $(A^{-1}) =$
AP ECET ME - 2025
AP ECET ECE - 2025
AP ECET Metallurgical Eng - 2025
AP ECET Mining Engg - 2025
Matrices and Determinants
View Solution