List of top Mineral Processing and Extractive Metallurgy Questions on Iron Making Mass Balance

A blast furnace produces hot metal with the following composition: 4 wt.% C, 1.5 wt.% Si, and the rest Fe.
The only input of iron is through iron ore containing 85 wt.% \(Fe_2O_3\) and 15 wt.% gangue consisting of \(SiO_2\) and \(Al_2O_3\).
2% of all the iron (by weight) is lost in the slag.
The amount of ore used to produce 1000 kg of hot metal (rounded off to one decimal place) is _________________ kg.
Given: Atomic weights of Fe and O are 56 g/mol and 16 g/mol, respectively.
  • GATE MT - 2026
  • GATE MT
  • Mineral Processing and Extractive Metallurgy
  • Iron Making Mass Balance