A low projection on the drag surface of a casting commencing near the gate by erosion of sand due to the high velocity liquid metal in the bottom gating. This defect is known as:
Show Hint
To eliminate wash defects:
- Adopt an unpressurized gating system design to decrease the fluid velocity.
- Elevate the sand's green/dry binding strength by adding appropriate clay and binder content.