An alloy having composition W-20 wt.% Ni is prepared by mixing elemental powders. The resulting powder mixture is liquid phase sintered at \(1550^{\circ}\text{C}\) for 1 hour. The liquid phase sintered microstructure consists of interconnected, spherical tungsten grains dispersed in nickel. The tungsten grain size is 70 \(\mu\text{m}\) and the W-W interparticle neck diameter is 35 \(\mu\text{m}\). If W-Ni interfacial energy is 0.30 J/m\(^2\), the W-W interfacial energy (in J/m\(^2\)), rounded off to two decimal places is ______.
(Given: melting point of W: \(3410^{\circ}\text{C}\) and melting point of Ni: \(1455^{\circ}\text{C}\))